Gemyske gearstalling:
Main en lytse komponinten | Min. ynhâld(%) | ASTM B760 |
W | 99.95 | lykwicht |
Unreinheden | Max.wearden (μg/g) | Max.wearden (μg/g) |
Al | 15 | - |
Cu | 10 | - |
Cr | 20 | - |
Fe | 30 | 100 |
K | 10 | - |
Ni | 20 | 100 |
Si | 20 | 100 |
Mo | 100 | - |
C | 30 | 100 |
H | 5 | - |
N | 5 | 100 |
O | 20 | 100 |
Cd | 5 | - |
Hg | 1 | - |
Pb | 5 | - |
Diameter en tolerânsjes:
Diameter (mm) | Tolerânsje | |||
Rjochte | Forged | Draaide | Grûn | |
0,50-0,99 | - | - | ±0.007 | |
1.00-1.99 | - | - | ±0.010 | |
2.00-2.99 | ±2.0 % | - | ±0.015 | |
3.00-15.9 | - | - | ±0.020 | |
16.0-24.9 | - | ±0.30 | ±0.030 | |
25.0-34.9 | - | ±0.40 | ±0.050 | |
35,0-39,9 | - | ±0.40 | ±0.30 | ±0.060 |
40,0-49,9 | - | ±0.40 | ±0.30 | ±0.20 |
50,0-90,0 | - | ±1.00 | ±0.40 | - |
Lingte en rjochtheid:
Diameter (mm) | Produksje lingte (mm) | Stiraightness / Meter (mm) | |
Cleaned | Grûn / draaide | ||
0,50-10,0 | ≥500 | <2.5 | <2.5 |
10,1-50,0 | ≥300 | <2.0 | <1.5 |
50,1-90,0 | ≥100 | <2.0 | <1.5 |
Lengte tolerânsje:
Diameter 0,50-30,0 mm | ||||||
Nominale lingte (mm) | ≥15 | 15-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Lengte tolerânsje (mm) | ±0,2 | ±0,3 | ±0,5 | ±2,0 | ±3,0 | ±4,0 |
Diameter >30,0 mm | ||||||
Nominale lingte (mm) | ≥30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Lengte tolerânsje (mm) | ±0,5 | ±0,8 | ±1.2 | ±4,0 | ±6,0 | ±8,0 |
Tichte: ≥19.1g/cm³
Net-destruktive testen: Foar diameters >15.00 mm: 100% ultrasone testen. Foar diameters fan 0.50-50.0mm: Eddy Curent testen op roeden mei grûn oerflak.
Diameter (mm) | Hardheid (HV 10) |
0,50-2,99 | - |
3.00-9.99 | 420-500 |
10.0-29.9 | 420-480 |
30,0-49,9 | 380-460 |
≥50 | >350 |
Oerflak betingst:
Diameter (mm) | Surface condition |
0,50-90,0 | Chemical skjinmakke |
≥40,0 | Draaide Ra ≤3.2μm |
0.50-30 | Centerless grûn Ra≤1.0μm |
≥40,0 | - Centerless grûn Ra≤1.2μm |