Special Price for 99.95% Pure Molybdenum Tzm Moly Rod/bar For Heating Furnace
Now we have highly developed devices. Our items are exported towards the USA, the UK and so on, enjoying a great popularity among the customers for Special Price for 99.95% Pure Molybdenum Tzm Moly Rod/bar For Heating Furnace, With the eternal goal of “continuous quality improvement, customer satisfaction”, we are sure that our product quality is stable and reliable and our products are best-selling at home and abroad.
Now we have highly developed devices. Our items are exported towards the USA, the UK and so on, enjoying a great popularity among the customers for 99.95% Pure Molybdenum, Molybdenum Tzm Moly Rod/bar, Tzm Moly Rod/bar For Heating Furnace, More than 26 years, Experienced companies from all over the world take us as their long-term and stable partners. We are keeping durable business relationship with more than 200 wholesalers in Japan, Korea, USA, UK, Germany, Canada, France, Italian, Poland, South Africa, Ghana, Nigeria etc.
TZM rods
Chemical composition:
Main and minor components | Min.content(%) | ASTM B386 (361) |
Mo | blance | balance |
Ti | 0.40-0.55% | 0.40-0.55% |
Zr | 0.06-0.12% | 0.06-0.12% |
Impurities | Max.values (μg/g) | Max.values (μg/g) |
Al | 10 | - |
Cu | 20 | - |
Cr | 20 | - |
Fe | 20 | 100 |
K | 20 | - |
Ni | 10 | 50 |
Si | 20 | 50 |
W | 300 | - |
C | 100-400 | 100-400 |
H | 10 | - |
N | 10 | 20 |
O | 500 | 300 |
Cd | 5 | - |
Hg | 1 | - |
Pb | 5 | - |
Dimensions and tolerances:
Diameter (mm) | Diameter tolerance (mm) |
Ground | |
0.50-0.99 | ±0.007 |
1.00-1.99 | ±0.010 |
1.00-2.99 | ±0.015 |
3.00-15.9 | ±0.020 |
16.0-24.9 | ±0.030 |
25.0-34.9 | ±0.050 |
35.0-3939 | ±0.060 |
≥40.0 | ±0.20 |
Cleaned | |
0.50-4.0 | ±2.0% |
4.10-10.0 | ±1.5% |
15.0-50.0 | ±0.30 |
51.0-75.0 | ±0.40 |
75.1-120.0 | ±1.00 |
121.0-165.0 | ±1.50 |
Turned | |
40.0-49.9 | ±0.30 |
50.0-165.0 | ±0.40 |
Length and straightness:
Diameter (mm) | Production length (mm) | Stiraightness/Meter (mm) | |
Cleaned | Ground/turned | ||
0.50-0.99 | >500 | <2.5 | <2.5 |
1.00-9.90 | >300 | <2.0 | <1.5 |
10.0-165.0 | >100 | <1.5 | <1.0 |
Length tolerance:
Diameter 0.50-30.0 mm | ||||||
Nominal length (mm) | 6-30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Length tolerance(mm) | ±0.2 | ±0.3 | ±0.5 | ±0.8 | ±1.2 | ±2.0 |
Diameter >30.0 mm | ||||||
Nominal length (mm) | 6-30 | 30-120 | 120-400 | 400-1000 | 1000-2000 | >2000 |
Length tolerance(mm) | ±1.0 | ±1.5 | ±2.5 | ±4.0 | ±6.0 | ±8.0 |
Density:
1. 0.50-40.0 mm ≥10.15g/cm³
2. 40.1-80.0 mm ≥10.10g/cm³
3. 80.1-120.0 mm ≥10.00g/cm³
4. 120.1-165.0 mm ≥9.90g/cm³
Nondestructive testing: For diameters>15.00 mm:100% ultrasonic testing; For diameters of 0.50-50.0mm:Eddy curent tests on rods with ground.
Diameter(mm) | Tensile strength(MPa) | 0.2% Yield Strength(MPa) | Elongation(%) | Hardness(HV 10) |
0.50-4.76 | - | - | - | - |
4.76-22.20 | ≥790 | ≥690 | ≥18 | |
22.20-28.60 | ≥760 | ≥655 | ≥15 | 260-320 |
28.60-47.60 | ≥690 | ≥585 | ≥10 | 250-310 |
47.60-73.00 | ≥620 | ≥550 | ≥10 | 245-300 |
73.00-120.9 | ≥585 | ≥515 | ≥5 | 240-290 |
121.0-165 | ≥585 | ≥515 | ≥5 | 220-280 |
Surface condition:
Surface: | Cleaned | Ground | Turned |
φ0.50-165mm | φ0.50-50.00mm | φ≥40.00mm | |
Roughness | Diameter (mm) | Ra (μm) Ground | Ra (μm) Turned |
≤2.50 | ≤0.80 | - | |
2.5-50.0 | ≤1.00 | - | |
≥40.0 | - | ≤3.2 |