Discount Price Astm B386 Tzm Molybdenum Sheet /plate

Short Description:


Product Detail

Product Tags

We intention to see quality disfigurement within the creation and supply the ideal support to domestic and overseas buyers wholeheartedly for Discount Price Astm B386 Tzm Molybdenum Sheet /plate, Our corporation warmly welcome good friends from everywhere in the earth to visit, investigate and negotiate organization.
We intention to see quality disfigurement within the creation and supply the ideal support to domestic and overseas buyers wholeheartedly for Astm B386 Moly Sheet/Plate, Heating Element Radiation Shield, Tzm Moly Sheet/Plate, Our production have been exported to more than 30 countries and regions as first hand source with lowest price. We sincerely welcome customers from both at home and abroad to come to negotiate business with us.
Chemical composition:

Main and minor components Min.content(%) ASTM B386 (361)
Mo Balance balance
Ti 0.40-0.55% 0.40-0.55%
Zr 0.06-0.12% 0.06-0.12%
Impurities Max.values (μg/g) Max.values (μg/g)
Al 10 -
Cu 20 -
Cr 20 -
Fe 20 100
K 20 -
Ni 10 50
Si 20 100
W 300 -
C 100-400 100-400-
H 10 -
N 10 20
O 500 300
Cd 5 -
Hg 1 -
Pb 5 -

Dimensions and tolerances:

Cold rolled sheets
Thickness(mm) Thickness tolerace(±mm) Maximal width(mm) Width tolerace(±mm)
0.30-0.50 0.028 300 1.0
Hot rolled sheets
Thickness(mm) Thickness tolerace(±mm) Maximal width(mm) Width tolerace(±mm)
0.50-0.60 0.06 850 1.6
0.60-1.00 0.08 850 1.6
1.00-1.50 0.13 850 2.0
1.50-2.00 0.15 850 2.0
2.00-3.60 0.18 850 2.0
3.60-50.0 5% 1000 2.0

Length tolerance:
The length tolerance for all dimension is maximal +5/-0 mm.
Flatness: max. 4 % (measuring procedure on the basis of ASTM B 386)
Density: ≥ 10.1 g/cm³
Vickers Hardness: 220-320 HV
Tensile Test:

Thickness (mm) Tensile StrengthMin. (MPa) 0.2% Yield strengtMin.(MPa) ElongationMin.(%)
0.30-1.00 700 600 5
1.00-2.50 700 600 10
2.50-5.00 700 600 12
5.00-20.00 650 600 10
20.00-50.00 550 470 5

Appearance: The material will be of uniform quality, free from foreign mater, splits and fractures. Bed sheet (not trimmed) may have small edge cracks.
Surface defedts are assessed in the frame of visual inspection.
Surface condition: pickled.


  • Previous:
  • Next:

  • Write your message here and send it to us